Stainless Steel Wire

stainless steel wire (3).jpg


Stainless Steel 304, like 302, has good mechanical properties and corrosion resistance.

Stainless Steel 304 is also known as AISI 304.


Chemical   Composition

SpecificationsDesignationsKey FeaturesTypical   Applications
ElementMin %Max %ASTM   A313
    ASTM A580
    BS 970
    BS 2056
W.NR   1.4301
    W.NR 1.4307
    UNS S30400
    AWS 161
Good   mechanical properties and corrosion resistance.Springs.
    Engineered components.
    Wire mesh.
    Wire cloth.
    Hose braiding.
C0.07
Mn2
P0.045
S0.03
Si1
Cr17.519.5
Ni810.5
FeBAL







Density8.0 g/cm30.289   lb/in3
Melting Point1454°C2650°F
Coefficient   of Expansion18.2   μm/m °C (20 – 100°C)10.1   x 10-6 in/in   °F (70 – 212°F)
Modulus of Rigidity70.3   kN/mm210196   ksi
Modulus of Elasticity187.5   kN/mm227195   ksi







Heat Treatment of   Finished Parts
Condition as supplied by Alloy WireTypeTemperatureTime   (Hr)Cooling
°C°F
Annealed   or Spring TemperStress   Relieve2504801Air







Properties
ConditionApprox.   tensile strengthApprox.   operating temperature
N/mm2ksi°C°F
Annealed600   – 80087   – 116-200   to +300-330   to +570
Spring   Temper1300   – 2200189   – 319-200   to +300-330   to +570


The above tensile strength ranges are typical. If you require different please ask.

stainless steel wire (4).jpg

Stainless Steel 316

Stainless Steel 316 has slightly better corrosion resistance than 302 and 304. It also has better non-magnetic properties.

Stainless Steel 316 is also known as AISI 316.



Chemical   Composition

SpecificationsDesignationsKey FeaturesTypical   Applications
ElementMin %Max %ASTM   A313
    ASTM A580
    BS 970
    BS 2056
W.NR   1.4401
    W.NR 1.4404
    UNS S31600
    AWS 162
Better   corrosion resistance and non-magnetic properties than 302 & 304   stainless.
    Better pitting and crevice corrosion resistance than 302 & 304   stainless.
More   suited to Marine, Food and Medical applications than
    302 and 304 stainless.
    Food processing
    Springs
    Engineered components.
    Wire mesh.
    Wire cloth
    Hose braiding
C0.07
Mn2
P0.045
S0.03
Si1
Cr1618.5
Ni9.513
Mo22.5







Density8.0 g/cm30.289   lb/in3
Melting Point1398°C2555°F
Coefficient   of Expansion 17.5 μm/m °C (20 – 100°C) 9.7 x 10-6 in/in °F (70 – 212°F)
Modulus of Rigidity 70.3 kN/mm2 10196 ksi
Modulus of Elasticity187.5   kN/mm227195   ksi







Heat Treatment of   Finished Parts
Condition as supplied by Alloy WireTypeTemperatureTime   (Hr)Cooling
°C°F
Annealed   or Spring TemperStress   Relieve2504801Air







Properties
ConditionApprox.   tensile strengthApprox.   operating temperature
N/mm2ksi°C°F
Annealed600   – 80087   – 116-200   to +300-330   to +570
Spring   Temper1300   – 2200189   – 319-200   to +300-330   to +570
The above tensile strength ranges are typical. If you require different please ask.